Some recent studies of material response have identified an issue that crosses over and blurs the boundary between ASME Boiler and Pressure Vessel Code Section III Subsection NB and Subsection NH. For very long design lives, the effects of creep show up at lower and lower temperature as the design life increases. Although true for the temperature at which the allowable stress is governed by creep properties, the effect is more apparent, e.g., creep effects show up sooner, at local structural discontinuities and peak thermal stress locations. This is because creep is a function of time, temperature, and stress, and the higher the localized stress, the lower in temperature creep begins to cause damage. If the threshold is below the Subsection NB to NH temperature boundary, for ferritic steels and for austenitic materials, then this potential failure mode will not be considered. Unfortunately, there is no experience base with very long lives at temperatures close to but under the Subsection NB to NH boundary to draw on. This issue is of particular interest in the application of Subsection NB rules of construction to some high temperature gas-cooled reactor concepts. The purpose of this paper is, thus, twofold: one part is about statistical treatment and extrapolation of sparse data for a specific material of interest, SA-533 Grade B Class 1; the other part is about how these results could impact current design procedures in Subsection NB.
Skip Nav Destination
e-mail: shamt@ornl.gov
Article navigation
January 2010
Research Papers
Creep Effects on Design Below the Temperature Limits of ASME Section III Subsection NB
T.-L. Sham,
e-mail: shamt@ornl.gov
T.-L. Sham
Fellow ASME
Oak Ridge National Laboratory
, 1 Bethel Valley Road, P.O. Box 2008, MS-6155, Oak Ridge, TN 37831-6155
Search for other works by this author on:
Robert I. Jetter,
Robert I. Jetter
Consultant
Fellow ASME
Pebble Beach, CA 93953
Search for other works by this author on:
Daniel R. Eno
Daniel R. Eno
Consultant
Guilderland, NY 12084
Search for other works by this author on:
T.-L. Sham
Fellow ASME
Oak Ridge National Laboratory
, 1 Bethel Valley Road, P.O. Box 2008, MS-6155, Oak Ridge, TN 37831-6155e-mail: shamt@ornl.gov
Robert I. Jetter
Consultant
Fellow ASME
Pebble Beach, CA 93953
Daniel R. Eno
Consultant
Guilderland, NY 12084
J. Eng. Gas Turbines Power. Jan 2010, 132(1): 012904 (6 pages)
Published Online: October 2, 2009
Article history
Received:
October 20, 2008
Revised:
November 24, 2008
Published:
October 2, 2009
Citation
Sham, T., Jetter, R. I., and Eno, D. R. (October 2, 2009). "Creep Effects on Design Below the Temperature Limits of ASME Section III Subsection NB." ASME. J. Eng. Gas Turbines Power. January 2010; 132(1): 012904. https://doi.org/10.1115/1.3126263
Download citation file:
Get Email Alerts
Cited By
Temperature Dependence of Aerated Turbine Lubricating Oil Degradation from a Lab-Scale Test Rig
J. Eng. Gas Turbines Power
Multi-Disciplinary Surrogate-Based Optimization of a Compressor Rotor Blade Considering Ice Impact
J. Eng. Gas Turbines Power
Experimental Investigations on Carbon Segmented Seals With Smooth and Pocketed Pads
J. Eng. Gas Turbines Power
Related Articles
Evaluation of the Creep Rupture Behavior of Alloy 690 Steam Generator Tubes Considering the Pressure Ramp Rate
J. Pressure Vessel Technol (February,2022)
The Creep and Stress-Rupture Testing of Steam-Boiler Materials
Trans. ASME (February,1952)
Design of Steam Piping and Valves for 1100 F
Trans. ASME (February,1954)
Serviceability Assessment of Creep Strength Enhanced Ferritic Steels
J. Pressure Vessel Technol (October,2015)
Related Proceedings Papers
Related Chapters
Basic Concepts
Design & Analysis of ASME Boiler and Pressure Vessel Components in the Creep Range
Polycrystalline Simulations of In-Reactor Deformation of Zircaloy-4 Cladding Tubes during Nominal Operating Conditions
Zirconium in the Nuclear Industry: 20th International Symposium
Division 5—High Temperature Reactors
Online Companion Guide to the ASME Boiler & Pressure Vessel Codes