The solderability of a wrought nickel pin directly overplated with gold and that of a wrought kovar (tradename of an Fe-Ni-Co alloy manufactured by Carpenter Technology Corporation) pin plated with thick nickel and then overplated with gold was evaluated. The kovar pin was determined to exhibit very high solderability whereas the nickel pin was found to have extremely poor solderability. The poor solderability of the nickel pin as compared with the kovar pin is attributed to the contamination of the nickel surface prior to gold plating. A primary cause of the poor wetability of the nickel pin was due to embedded alumina particles on the surface of the pin (this occurs during the tumbling operation to remove any metallic slivers) prior to gold plating. The high solderability of the kovar is related to the clean nickel plating prior to overplating with gold. The cleanliness of the nickel layer was found to strongly influence the formation of the Ni-Sn intermetallic phase layer, having a nominal thickness of 42 μin (1.1 μm) after the kovar pin was tinned with eutectic Sn-Pb solder. For the tinned wrought nickel pin, a thin but continuous Ni-Sn intermetallic layer was also present; however, the nominal thickness of this layer was only 15 μin (0.38 μm). This large variation in solderability of both types of pins is attributed to differences in the intermetallic phase layer.
Skip Nav Destination
Article navigation
September 1990
Research Papers
A Comparison of the Solderability of Wrought and Plated Nickel Surfaces: The Selection of a Reliable Pin for Second Level Packaging
C. G. Woychik,
C. G. Woychik
IBM Corporation, Endicott, NY 13760
Search for other works by this author on:
A. K. Trivedi
A. K. Trivedi
IBM Corporation, Endicott, NY 13760
Search for other works by this author on:
C. G. Woychik
IBM Corporation, Endicott, NY 13760
A. K. Trivedi
IBM Corporation, Endicott, NY 13760
J. Electron. Packag. Sep 1990, 112(3): 223-233 (11 pages)
Published Online: September 1, 1990
Article history
Received:
September 1, 1989
Revised:
April 2, 1990
Online:
April 28, 2008
Article
Article discussed|
View article
Connected Content
A commentary has been published:
Closure to “Discussion of ‘On Stick-Slip and Velocity Dependence of Friction at Low Speeds’” (1991, ASME J. Tribol., 113, p. 223)
Citation
Woychik, C. G., and Trivedi, A. K. (September 1, 1990). "A Comparison of the Solderability of Wrought and Plated Nickel Surfaces: The Selection of a Reliable Pin for Second Level Packaging." ASME. J. Electron. Packag. September 1990; 112(3): 223–233. https://doi.org/10.1115/1.2904371
Download citation file:
Get Email Alerts
Cited By
Sequential Versus Concurrent Effects in Combined Stress Solder Joint Reliability
J. Electron. Packag
Anand Model Constants of Sn-Ag-Cu Solders: What Do They Actually Mean?
J. Electron. Packag
Related Articles
Cracking of the Intermetallic Compound Layer in Solder Joints Under Drop Impact Loading
J. Electron. Packag (September,2011)
Influence of Intermetallic Characteristics on the Solder Joint Strength of Halogen-Free Printed Circuit Board Assembly
J. Electron. Packag (June,2011)
Optimized Design of Various Ag Decorated Sn-xAg-Cu 0.7 Solder Bump on Cycling Fatigue Reliability for Wafer-Level Chip Scale Packaging
J. Electron. Packag (December,2022)
Wetting Kinetics of Molten 60Sn40Pb on a Ag-0.33 wt.% Pt Thick Film Conductor
J. Electron. Packag (September,1995)
Related Proceedings Papers
Related Chapters
Dismantling
Decommissioning Handbook
Structural Evolutions of Nanocrystalline Nial Evtermetallic during Mechanical Alloying Process
International Conference on Mechanical and Electrical Technology, 3rd, (ICMET-China 2011), Volumes 1–3
A Study of Irradiation-Induced Growth of Modified and Advanced Zr-Nb System Alloys after Irradiation in the VVER-1000 Reactor Core at Temelin NPP
Zirconium in the Nuclear Industry: 20th International Symposium